Abstract:The “cement-to-asphalt” overlay technique can fully utilize the residual strength of the existing pavement and improve the ride comfort, which has become one of the mainstream solutions for the reconstruction of cement pavements. Relying on an expressway project in Guangxi, the technical condition and defect characteristics of the original cement pavement are systematically analyzed through field inspections and laboratory tests, including the pavement condition index (PCI), riding quality index (RQI), joint load-carrying capacity, and cavity beneath the slabs. The results indicate that the defects on the carriageway are significantly more severe than on the passing lanes. The broken slabs, cracks, exposed aggregate and strip-shaped patches are the primary types of defects. Additionally, the equivalent modulus of elasticity at the base course surface is relatively low. Combined with traffic load analysis, the cumulative equivalent axle load count on the mainline has exceeded the extra-heavy traffic class specified for the original design service life. Based on this, the technical characteristics, construction difficulty and economic viability of different combinations of stress-absorbing layers and asphalt surface courses are compared. The recommended overlay structure is a “2.5 cm SBS-modified asphalt AC-10 stress-absorbing layer + 4 cm SBS-modified asphalt SMA-13,” which provides a technical reference for similar renovation projects involving old cement pavements.